This paper is to investigate the spalling resistance and fire endurance of high performance concrete with the kinds of contents of fiber. According to test results. plain concrete without fiber exhibited severe spalling failure subjected to fire for 3 hours. However, the use of PP fiber had an effect on preventing spalling by discharging internal vapour pressure. Although the use of CL fiber shows better fire resistance than plain concrete. some failure was observed at the corner of specimens. Residual strength after fire test showed 20% in plain concrete, 40% in PP fiber concrete and 25% in CL fiber concrete. The proper contents of PP fiber is found to be 0.9㎏/m3 based on the results of fire test in the side of mass loss, spalling depth and occurrence area of spalling. The neutralization depth of concrete after fire resistance test was shown to be 8㎜.

목차

Abstract
1. 서론
2. 실험계획 및 방법
3. 실험결과 및 분석
4. 결론
참고문헌

참고문헌 (0)

참고문헌 신청

함께 읽어보면 좋을 논문

논문 유사도에 따라 DBpia 가 추천하는 논문입니다. 함께 보면 좋을 연관 논문을 확인해보세요!

이 논문의 저자 정보

이 논문과 함께 이용한 논문

최근 본 자료

전체보기

댓글(0)

0

UCI(KEPA) : I410-ECN-0101-2009-540-016517131