오류제보하기
This study was performed to investigate the reaction between alkylketene dimer(AKD) and cellulose molecules in AKD-sized paper sheet. AKD was added to highly beaten (80±3°SR) SwBKP (ca. 0.8%on pulp) in order to have much AKD retention in the paper sheet. This AKD-sized paper sheet was aged at different temperatures, 60℃, 80℃, 105℃ and 125℃. Changes in FT-IR spectra of AKD in paper sheet during the ageing were measured. In addition, sizing degrees of the AKD-sized paper sheet pretreated for 30 sec. at 105℃ were measured by HST size tester during the storage at different temperature. IR spectra of AKD-sized paper sheet preheated at 105℃ for 30 sec. showed unchanged spectra two absorption bands at 1849 ㎝<SUP>-1</SUP> and 1722 ㎝<SUP>-1</SUP> which refer to the typical AKD IR bands. However, these typical AKD bands were gradually reduced with increasing ageing, completely disappeared after 6 hrs. and formed new absorption band at 1706 ㎝<SUP>-1</SUP>, which refers to carbonyl stretching vibration of dialkylktone. Eventually the AKD molecule was hydrolyzed to diakylketone without formation of -ketoester with cellulose in paper sheet. After 6 days ageing, a little amount of -ketoester bands was identified in 6 or 7 days ageing, because of the absence of water due to long-term heating. The same tendency was observed at different ageing conditions. At the practical papermaking process, AKD reacts prevailing with water, and mostly seems to be hydrolyzed to dialkylketene.
Concerned to the sizing development, AKD-sized paper sheet was shown no sizing development at the initial stage of ageing at 60℃ after heating treatment at 105℃ for 30 sec., and gradually increased the sizing degree with increasing ageing, such as Hercules Sizing Tester (HST) 130 sec for 12 hr, HST 300 sec. for 3 days and HST 400 sec. for 5 days. It was concluded that hydrolyzed AKD could contributed to the sizing development of the paper sheet.

목차

ABSTRACT
1. TJFHS
2. 재료 및 방법
3. 결과 및 고찰
4. 결론
인용문헌

참고문헌 (0)

참고문헌 신청

함께 읽어보면 좋을 논문

논문 유사도에 따라 DBpia 가 추천하는 논문입니다. 함께 보면 좋을 연관 논문을 확인해보세요!

이 논문의 저자 정보

이 논문과 함께 이용한 논문

최근 본 자료

전체보기

댓글(0)

0

UCI(KEPA) : I410-ECN-0101-2009-586-016573273