The main objective of this study was to evaluate the effects on shape and size, compressive strength, water absorption and heavy metals leaching with various weight mixing ratios in waste ash brick products using waste recycling MSWI(Municipal Solid Waste Incinerator) bottom ash, steel slag and waste building material. The manufacturing processes for the waste ash brick consist of screening, mixing, conveyor transmission, compaction·forming, and curing steps of raw materials. The weight mixing ratios of steel slag around bottom ash were adjusted within the ranges of 10% to 30%. The reported results show that the width and thickness of the manufactured waste ash brick could be satisfied with 90 ± 2 mm and 57 ± 2 mm, respectively which are K.S. standards of products qualities. And in case of length, only 20-Ba50Ss30, 20-Ba60Wb20 and 20-Ba50Wb30 for the mixing ratios could be satisfied with 190 ± 2 mm that is K.S. standards of products quality. The compressive strength and water absorption for 20-Ba50Ss30 and 20-Ba70Wb10 were over 8 N/mm2 and below 15% respectively that are K.S. standards of manufactured waste ash brick. The results of tests for the heavy metals leaching in the all manufactured waste ash bricks are also passed to the wastes management regulations. The cost analysis of 20-Ba50Ss30 is evaluated. The manufacturing cost is evaluated 34.3 won/brick with 8 hours and 20tons of raw material per day. Incinerators with problems in bottom ash disposal can therefore derive significant benefits from the application of waste ash brick production.

목차

등록된 정보가 없습니다.

참고문헌 (29)

참고문헌 신청

함께 읽어보면 좋을 논문

논문 유사도에 따라 DBpia 가 추천하는 논문입니다. 함께 보면 좋을 연관 논문을 확인해보세요!

이 논문의 저자 정보

최근 본 자료

전체보기

댓글(0)

0