메뉴 건너뛰기
.. 내서재 .. 알림
소속 기관/학교 인증
인증하면 논문, 학술자료 등을  무료로 열람할 수 있어요.
한국대학교, 누리자동차, 시립도서관 등 나의 기관을 확인해보세요
(국내 대학 90% 이상 구독 중)
로그인 회원가입 고객센터 ENG
주제분류

추천
검색

논문 기본 정보

자료유형
학술저널
저자정보
Sareh Habibzadeh (Tehran University of Medical Sciences International Campus School of Dentistry Tehran Iran) Hamid Reza Rajati (Faculty of Dentistry Mashhad University of Medical Sciences Mashhad Iran) Habib Hajmiragha (Tehran University of Medical Sciences School of Dentistry Tehran Iran) Shima Esmailzadeh (Tehran University of Medical Sciences International Campus School of Dentistry Tehran Iran) Mohamadjavad Kharazifard (Dental Research Center Tehran University of Medical Sciences Tehran Iran)
저널정보
대한치과보철학회 The Journal of Advanced of Prosthodontics The Journal of Advanced of Prosthodontics 제9권 제3호
발행연도
2017.6
수록면
170 - 175 (6page)
DOI
https://doi.org/10.4047/jap.2017.9.3.170

이용수

표지
📌
연구주제
📖
연구배경
🔬
연구방법
🏆
연구결과
AI에게 요청하기
추천
검색

초록· 키워드

오류제보하기
PURPOSE. The aim of the present study was to evaluate the fracture resistances of zirconia, cast nickel-chromium alloy (Ni-Cr), and fiber-composite post systems under all-ceramic crowns in endodontically treated mandibular first premolars. MATERIALS AND METHODS. A total of 36 extracted human mandibular premolars were selected, subjected to standard endodontic treatment, and divided into three groups (n=12) as follows: cast Ni-Cr post-and-core, one-piece custom-milled zirconia post-and-core, and prefabricated fiber-glass post with composite resin core. Each specimen had an all-ceramic crown with zirconia coping and was then loaded to failure using a universal testing machine at a cross-head speed of 0.5 mm/min, at an angle of 45 degrees to the long axis of the roots. Fracture resistance and modes of failure were analyzed. The significance of the results was assessed using analysis of variance (ANOVA) and Tukey honest significance difference (HSD) tests (α=.05). RESULTS. Fiber-glass posts with composite cores showed the highest fracture resistance values (915.70±323 N), and the zirconia post system showed the lowest resistance (435.34±220 N). The corresponding mean value for the Ni-Cr casting post and cores was reported as 780.59±270 N. The differences among the groups were statistically significant (P<.05) for the zirconia group, as tested by ANOVA and Tukey HSD tests. CONCLUSION. The fracture resistance of zirconia post-and-core systems was found to be significantly lower than those of fiberglass and cast Ni-Cr post systems. Moreover, catastrophic and non-restorable fractures were more prevalent in teeth restored by zirconia posts.